In this study, the optimization of dissolution in the gluconic acid solutions of magnesite ore was performed according to Taguchi method. In the process of dissolution, particle size, acid concentration, solid to liquid ratio, stirring speed and reaction temperature as parameter were chosen. Optimum conditions for the maximum dissolution of magnesite ore are determined by using performance statistics of “the bigger – the better” by Taguchi Method. The optimum conditions that a conversion of 99.9 % was achieved were determined as particle size -80+120 mesh, solid-liquid ratio 1/35 g.mL-1, reaction temperature 80oC, reaction period 90 minute and acid concentration 1.25 M. Hence, it can be said that the optimization results are within 95% confidence level
Bu çalışmada, ham manyezitin glukonik asit çözeltilerinde çözündürülmesinin Taguchi metoduna göre optimizasyonu incelenmiştir. Asit konsantrasyonu, reaksiyon süresi, katı/sıvı oranı, partikül boyutu ve reaksiyon sıcaklığı gibi parametrelerin etkisi incelenmiştir. Taguchi’nin“En yüksek-en iyi” performans istatistiği uygulanarak maksimum manyezit dönüşümünün gerçekleştiği optimum şartlar belirlenmiştir. %98.79’luk maksimum manyezit dönüşümün elde edildiği optimum şartlar: asit konsantrasyonu 1,25 M, reaksiyon süresi 90 dakika, reaksiyon sıcaklığı 80oC, katı-sıvı oranı 1/35 g/mL ve tane boyutu -80 +120 mesh olarak tespit edilmiştir. %95 güven seviyesinde yapılan optimizasyonun doğru olduğu belirlenmiştir.
Primary Language | Turkish |
---|---|
Journal Section | Articles |
Authors | |
Publication Date | November 13, 2015 |
Published in Issue | Year 2015 Volume: 16 Issue: 2 |