Rehabilitation of a Severely Worn Dentition with Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report
Abstract
Rehabilitation of worn dentition is a challenging task because several predisposing factors may be included in the pathogenesis. The treatment options and process should be carefully considered based on the clinical condition and patients’ requirements. This case report represents the esthetic rehabilitation of a 68-year-old patient who exhibited severely worn teeth caused by attrition and erosion. After clinical evaluation, 3 mm increase in occlusal vertical dimension was planned with partial lithium-disilicate ceramic restorations as laminate veneers for anterior teeth and vonlays (onlays with veneer extentions) for posterior teeth in maxilla. The adaptation of the patient to the increased occlusal vertical dimension was tested for 1 month by provisional direct composite restorations. As the patient did not show any discomfort, definitive restorations were completed. The patient was satisfied with the esthetics and functionality of her new dentition.
Keywords
References
- 1. Alqahtani F. Full-mouth rehabilitation of severely worn dentition due to soda swishing: a clinical report. J Prosthodont. 2014;23(1):50-7.
- 2. Maroulakos G, Nagy WW, Stathopoulou PG, Mattheos N, Chronopoulos V. Restoration of the worn dentition: basic prosthodontic principles and current rehabilitation techniques. Curr Oral Health Rep. 2017;4(2):124-30.
- 3. Van't Spijker A, Rodriguez JM, Kreulen CM, Bronkhorst EM, Bartlett DW, Creugers NH. Prevalence of tooth wear in adults. Int J Prosthodont. 2009;22(1):35-42.
- 4. Vailati F, Belser UC. Full-mouth adhesive rehabilitation of a severely eroded dentition: the three-step technique. Part 1. Eur J Esthet Dent. 2008;3(1):30-44.
- 5. Bahillo J, Jané L, Bortolotto T, Krejci I, Roig M. Full-mouth composite rehabilitation of a mixed erosion and attrition patient: a case report with v-shaped veneers and ultra-thin CAD/CAM composite overlays. Quintessence Int. 2014;45(9):749-56.
- 6. Kaidonis JA, Richards LC, Townsend GC, Tansley GD. Wear of human enamel: a quantitative in vitro assessment. J Dent Res. 1998;77(12):1983-90.
- 7. Al-Salehi SK. Restorative Management of Intrinsic and Extrinsic Dental Erosion. J Indian Prosthodont Soc. 2014;14(Suppl 1):215-21.
- 8. Bettie NF, Kandasamy S, Prasad V. Management of tooth surface loss of varying etiology with full mouth all ceramic Computer-Aided Design/Computer-Aided Manufacture restorations. J Pharm Bioallied Sci. 2017;9(Suppl 1):S302-s5.
Details
Primary Language
English
Subjects
Dentistry
Journal Section
Case Report
Publication Date
April 30, 2021
Submission Date
March 26, 2021
Acceptance Date
April 11, 2021
Published in Issue
Year 2021 Volume: 48 Number: 1
APA
Oğuz, E. İ., & Berksun, S. (2021). Rehabilitation of a Severely Worn Dentition with Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report. European Annals of Dental Sciences, 48(1), 28-32. https://doi.org/10.52037/eads.2021.0009
AMA
1.Oğuz Eİ, Berksun S. Rehabilitation of a Severely Worn Dentition with Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report. EADS. 2021;48(1):28-32. doi:10.52037/eads.2021.0009
Chicago
Oğuz, Ece İrem, and Semih Berksun. 2021. “Rehabilitation of a Severely Worn Dentition With Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report”. European Annals of Dental Sciences 48 (1): 28-32. https://doi.org/10.52037/eads.2021.0009.
EndNote
Oğuz Eİ, Berksun S (April 1, 2021) Rehabilitation of a Severely Worn Dentition with Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report. European Annals of Dental Sciences 48 1 28–32.
IEEE
[1]E. İ. Oğuz and S. Berksun, “Rehabilitation of a Severely Worn Dentition with Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report”, EADS, vol. 48, no. 1, pp. 28–32, Apr. 2021, doi: 10.52037/eads.2021.0009.
ISNAD
Oğuz, Ece İrem - Berksun, Semih. “Rehabilitation of a Severely Worn Dentition With Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report”. European Annals of Dental Sciences 48/1 (April 1, 2021): 28-32. https://doi.org/10.52037/eads.2021.0009.
JAMA
1.Oğuz Eİ, Berksun S. Rehabilitation of a Severely Worn Dentition with Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report. EADS. 2021;48:28–32.
MLA
Oğuz, Ece İrem, and Semih Berksun. “Rehabilitation of a Severely Worn Dentition With Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report”. European Annals of Dental Sciences, vol. 48, no. 1, Apr. 2021, pp. 28-32, doi:10.52037/eads.2021.0009.
Vancouver
1.Ece İrem Oğuz, Semih Berksun. Rehabilitation of a Severely Worn Dentition with Partial Lithium-Disilicate Glass Ceramic Restorations: A Case Report. EADS. 2021 Apr. 1;48(1):28-32. doi:10.52037/eads.2021.0009