WC-Ni sert dolgu alaşımının kuru ve NaCl çözelti ortamlarındaki aşınma performansı
Öz
Anahtar Kelimeler
References
- Balakrishnan, M., Balasubramanian, V., Reddy, G.M., (2013). Effect of hardfacing consumables on ballistic performance of Q&T steel joints, Defence Technology, 9(4), 249-258.
- Buchanan, V.E., McCartney, D.G., Shipway, P.H., (2008). A comparison of the abrasive wear behaviour of iron-chromium based hardfaced coatings deposited by SMAW and electric arc spraying, Wear, 264(7-8), 542-549.
- Buchanan, V.E., Shipway, P.H., McCartney, D.G., (2007). Microstructure and abrasive wear behaviour of shielded metal arc welding hardfacings used in the sugarcane industry, Wear, 263(1-6), 99-110.
- Buchely, M.F., Gutierrez, J.C., Leon, L.M., Toro, A., (2005). The effect of microstructure on abrasive wear of hardfacing alloys, Wear, 259(1-6), 52-61.
- Buytoz, S., Orhan, A., Gur, A. K., Caligulu, U. (2013). Microstructural Development of Fe–Cr–C and B4C Powder Alloy Coating on Stainless Steel by Plasma-Transferred Arc Weld Surfacing. Arabian Journal for Science and Engineering, 38(8), 2197-2204.
- Chaidemenopoulos, N.G., Psyllaki, P.P., Pavlidou, E., Vourlias, G., (2019). Aspects on carbides transformations of Fe-based hardfacing deposits, Surface and Coatings Technology, 357, 651-661.
- Deng, D., Zhang, L., Niu, T., Liu, H., Zhang, H., (2015). Microstructures and wear performance of PTAW deposited Ni-based coatings with spherical tungsten carbide, Metals, 5(4), 1984-1996.
- Hajihashemi, M., Shamanian, M., Azimi, G., (2015). Physical, Mechanical, and Dry Sliding Wear Properties of Fe-Cr-WC Hardfacing Alloys Under Different Tungsten Addition, Metallurgical and Materials Transactions B, 46(2), 919-927.
Details
Primary Language
Turkish
Subjects
-
Journal Section
Research Article
Authors
Nilay Çömez
*
0000-0002-6432-6582
Türkiye
Publication Date
June 15, 2020
Submission Date
February 19, 2019
Acceptance Date
April 2, 2019
Published in Issue
Year 2020 Volume: 11 Number: 2