Özet Yapılmış olan çalışmada; Cimara, Monobond-S, Silis-tor, Scotchprime, Clearfîl Activator ve Porcelain Anahtar sözcükler: Seramik tamir materyali, silan bağlayıcı materyal, seramik. Abstract The aim of this research was to detertnine the bond strength values of VMK 68 ceramic material to ceramic repair materials, trade named as Cimara, Monobond-S, Silistor, Scotc-hbond, Clearfil activator and Porcelain repair primer. The changes in the bond strength values related to time were also evaluated. Each repair system were applied to the samples and all tlie samples were left in 37"C water and had ther-mocycling before force application. Shearing force was applied to 10 samples of each system after 30 days. At the end of 1 and 30 days the kigliest bond strength values were obtained with Scotchbond followed by Silistor, Porcelain repair primer, Clearfil activator, Cimara and Monobond S in decreasing order. The results were evaluated using t tests for paired samples. According to the results there was a significant increase in the bond strenght value of Silistor porcelain repair material at the end of 30 days. On the other hand mere was a significant decrease in Monobond-S and Porcelain repair primer systems at tfte end 30 days. ScoctcJtbond and Clearfil activator systems have also displayed similar bond strenth values. Key words: Ceramic repair material, silane coupling agent, dental ceramic.
Primary Language | Turkish |
---|---|
Journal Section | Original Research Articles |
Authors | |
Publication Date | January 10, 2013 |
Published in Issue | Year 1997 Volume: 31 Issue: 4 |