In this study, AISI 2205 duplex stainless steel which has the widest usage area in its own category and, both higher welding capability and lower carbonaceous AISI 1020 steel pair providing with affordable price advantage is joined with continuous drive friction welding which is one of the solid-state methods by using different treatment parameters ( 1300, 1500, and 1700 rpm rotation speed, 4, 6, and 8 s friction time, and 40 MPa friction pressure).For microstructure examination, SEM analyse method are examined so as to determine amendments which will be able to occur in the interface of merger. it was determined with microstructure amendments in the joint interworking by completing micro hardness measurements perpendicular to the joint interface. It was aimed to examine the damage processes by executing tension test to the welded joints.
Bu çalışmada, kendi sınıfında en yaygın kullanım alanına sahip AISI 2205 dubleks paslanmaz çelik ile kaynak kabiliyeti yüksek ve aynı zamanda uygun fiyat avantajna sahip düşük karbonlu AISI 1020 çelik çifti farklı işlem parametreleri (1300, 1500 ve 1700 rpm devir sayısı, 4, 6 ve 8 s sürtünme süresi ve 40 MPa sürtünme basıncı) kullanılarak katı hal kaynak yöntemlerinden biri olan sürekli tahrikli sürtünme kaynağı ile birleştirilmiştir. Elde edilen bu kaynaklı bağlantıların birleşme arayüzeyinde meydana gelen değişiklikler SEM analizi ile belirlenmiştir. Kaynaklı bağlantılara çekme testi uygulanarak hasar süreçlerinin incelenmiş olup, bağlantı arayüzeyine dik doğrultuda mikrosertlik ölçümleri yapılmıştır.
Primary Language | Turkish |
---|---|
Journal Section | Electrical Machines |
Authors | |
Publication Date | March 1, 2013 |
Published in Issue | Year 2013 Volume: 8 Issue: 2 |