BibTex RIS Cite

TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ

Year 2009, Volume: 2009 Issue: 2, 98 - 104, 01.02.2009
https://izlik.org/JA44PW26NH

Abstract

-

References

  • Al-Wahadni A, an in vitro investigation into the surface roughness of 2 glazed, unglazed, and refinished ceramic materials, Quint Int 2006; 37(4):311-7
  • Kawai K, Urano M, Adherance of plaque components to different restorative materials, Operative Dent 2001, 26:396-400
  • Al-Wahadni A, Martin DM, Glazing and finishing dental porcelain: A literature review, JCDA 1998, 64:580-583
  • Gomis JM, Bizar J, Anglada JM, Samso J, Peraire M , Comparative evaluation of four finishing systems on one ceramic surface, Int J Prosthodont 2003, 16(1):74-77
  • Üçtaşlı S, Ergun G, Korkmaz T, Güllü A, Geleneksel ve düşük ısı porselenlerinin, glaze veya cilalama pürüzlülüğünün değerlendirilmesi, A.Ü. Diş Hek Fak Derg 2002; 29(1): 73-80 sonra yüzey
  • Apholt W, Bındl A, Luthy H, Mormann WH, Flexural strength of Cerec 2 machined and jointed In Ceram-Alumina ve In Ceram-Zirconia bars. Dent Mater 2001, 17:260-7
  • Aykent F, İnan Ö, Üşümez A, Sevimay M, Farklı polisaj yöntemleri uygulanan seramiklerde yüzey pürüzlülüğünün incelenmesi, G.Ü. Dişhek Fak Derg 2001; 18(2):63-67
  • Scurria MS, Powers JM , Surface roughness of two polished ceramic materials, J Prosthet Dent 1994, 71: 174-177
  • Sasahara RMC, Ribeiro FC, Cesar PH, Yoshimura HN, Influence of the finishing technique on surface roughness of dental porcelains with different microstructures, Oper Dent 2006, 31(5): 577-83
  • Jung M, Finishing and polishing of a hybrid composite and a heat-pressed glass ceramics, Oper Dent 2002, 27:175-183
  • Smith GA, Wilson NHF, The surface finish of trimmed porcelain, Br Dent J 1981, 151: 222- 24
  • Goldstein GR, Barnhard BR, Penugonda B, Profilometer, SEM and visual asessment of porcelain polishing methods, J Prosthet Dent 1991, 65:627-34
  • Hulterström AK, Bergman M, Polishing systems for dental ceramics, Acto Odontol Scand 1993, 51: 229-234
  • Gomis JM, Bizar J, Anglada JM, Samso J, Peraire M, Comparative evaluation of four finishing systems on one ceramic surface, Int J Prosthodont 2003, 16(1):74-77
  • Bessing C, Wiktorsson A, Comparison of two different methods of polishing porcelain, Scand J Dent Res 1983, 91:482-487
  • Sarac D, Sarac S, Yuzbasıoglu E, Bal A, The effects of porcelain polishing systems on the color and surface texture of feldspathic porcelain, J Prosthet Dent 2006, 96:122-8
  • Jagger DC, Harisson A, An in-vitro investigation into the wear effect of unglazed, glazed and polished porcelain on human dental enamel, J Prosthet Dent 1994; 72: 320- 323
  • Jung M, Wehlen O, Klimek J, Finishing and polishing of indirect composite and ceramic inlays in-vivo: occlusal surfaces, Oper Dent 2004, 29(2):131-41
  • Goldstein RE , Finishing composite and laminates, Dent Clinics North Am 1989, 33:305-18
  • Wright MD, Masri R, Driscoll CF, Romberg E, Thomson GA, Runyan DA, Comparison of three systems for the polishing of an ultra-low fusing dental porcelain, J Prosthet Dent 2004; 92:486- 490
  • Shillingburg HT, Hobo S, Whitsett LD, Fundamentals of Fixed Prosthodontics. 9th edd Quintessence Publishing Co 1997, Chicago
  • Kedici S, Tam seramikler, TDBD 2002,71: 78-80

TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ

Year 2009, Volume: 2009 Issue: 2, 98 - 104, 01.02.2009
https://izlik.org/JA44PW26NH

Abstract

Amaç: Bu çalışmanın amacı; beş farklı metal desteksiz seramik sistemine (IPS Empress, IPS Empress 2, In-Ceram (Vitadur Alpha), Vita Mark II ve Finesse) 4 farklı yüzey bitim ve polisaj işlemi uygulanmasının karşılaştırmalı olarak değerlendirmektir. yüzey pürüzlülüğüne etkisini

References

  • Al-Wahadni A, an in vitro investigation into the surface roughness of 2 glazed, unglazed, and refinished ceramic materials, Quint Int 2006; 37(4):311-7
  • Kawai K, Urano M, Adherance of plaque components to different restorative materials, Operative Dent 2001, 26:396-400
  • Al-Wahadni A, Martin DM, Glazing and finishing dental porcelain: A literature review, JCDA 1998, 64:580-583
  • Gomis JM, Bizar J, Anglada JM, Samso J, Peraire M , Comparative evaluation of four finishing systems on one ceramic surface, Int J Prosthodont 2003, 16(1):74-77
  • Üçtaşlı S, Ergun G, Korkmaz T, Güllü A, Geleneksel ve düşük ısı porselenlerinin, glaze veya cilalama pürüzlülüğünün değerlendirilmesi, A.Ü. Diş Hek Fak Derg 2002; 29(1): 73-80 sonra yüzey
  • Apholt W, Bındl A, Luthy H, Mormann WH, Flexural strength of Cerec 2 machined and jointed In Ceram-Alumina ve In Ceram-Zirconia bars. Dent Mater 2001, 17:260-7
  • Aykent F, İnan Ö, Üşümez A, Sevimay M, Farklı polisaj yöntemleri uygulanan seramiklerde yüzey pürüzlülüğünün incelenmesi, G.Ü. Dişhek Fak Derg 2001; 18(2):63-67
  • Scurria MS, Powers JM , Surface roughness of two polished ceramic materials, J Prosthet Dent 1994, 71: 174-177
  • Sasahara RMC, Ribeiro FC, Cesar PH, Yoshimura HN, Influence of the finishing technique on surface roughness of dental porcelains with different microstructures, Oper Dent 2006, 31(5): 577-83
  • Jung M, Finishing and polishing of a hybrid composite and a heat-pressed glass ceramics, Oper Dent 2002, 27:175-183
  • Smith GA, Wilson NHF, The surface finish of trimmed porcelain, Br Dent J 1981, 151: 222- 24
  • Goldstein GR, Barnhard BR, Penugonda B, Profilometer, SEM and visual asessment of porcelain polishing methods, J Prosthet Dent 1991, 65:627-34
  • Hulterström AK, Bergman M, Polishing systems for dental ceramics, Acto Odontol Scand 1993, 51: 229-234
  • Gomis JM, Bizar J, Anglada JM, Samso J, Peraire M, Comparative evaluation of four finishing systems on one ceramic surface, Int J Prosthodont 2003, 16(1):74-77
  • Bessing C, Wiktorsson A, Comparison of two different methods of polishing porcelain, Scand J Dent Res 1983, 91:482-487
  • Sarac D, Sarac S, Yuzbasıoglu E, Bal A, The effects of porcelain polishing systems on the color and surface texture of feldspathic porcelain, J Prosthet Dent 2006, 96:122-8
  • Jagger DC, Harisson A, An in-vitro investigation into the wear effect of unglazed, glazed and polished porcelain on human dental enamel, J Prosthet Dent 1994; 72: 320- 323
  • Jung M, Wehlen O, Klimek J, Finishing and polishing of indirect composite and ceramic inlays in-vivo: occlusal surfaces, Oper Dent 2004, 29(2):131-41
  • Goldstein RE , Finishing composite and laminates, Dent Clinics North Am 1989, 33:305-18
  • Wright MD, Masri R, Driscoll CF, Romberg E, Thomson GA, Runyan DA, Comparison of three systems for the polishing of an ultra-low fusing dental porcelain, J Prosthet Dent 2004; 92:486- 490
  • Shillingburg HT, Hobo S, Whitsett LD, Fundamentals of Fixed Prosthodontics. 9th edd Quintessence Publishing Co 1997, Chicago
  • Kedici S, Tam seramikler, TDBD 2002,71: 78-80
There are 22 citations in total.

Details

Primary Language Turkish
Authors

Dr. Dt. Neslihan Çökük This is me

Publication Date February 1, 2009
IZ https://izlik.org/JA44PW26NH
Published in Issue Year 2009 Volume: 2009 Issue: 2

Cite

APA Çökük, D. D. N. (2009). TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi, 2009(2), 98-104. https://izlik.org/JA44PW26NH
AMA 1.Çökük DDN. TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi. 2009;2009(2):98-104. https://izlik.org/JA44PW26NH
Chicago Çökük, Dr. Dt. Neslihan. 2009. “TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ”. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi 2009 (2): 98-104. https://izlik.org/JA44PW26NH.
EndNote Çökük DDN (February 1, 2009) TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi 2009 2 98–104.
IEEE [1]D. D. N. Çökük, “TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ”, Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi, vol. 2009, no. 2, pp. 98–104, Feb. 2009, [Online]. Available: https://izlik.org/JA44PW26NH
ISNAD Çökük, Dr. Dt. Neslihan. “TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ”. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi 2009/2 (February 1, 2009): 98-104. https://izlik.org/JA44PW26NH.
JAMA 1.Çökük DDN. TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi. 2009;2009:98–104.
MLA Çökük, Dr. Dt. Neslihan. “TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ”. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi, vol. 2009, no. 2, Feb. 2009, pp. 98-104, https://izlik.org/JA44PW26NH.
Vancouver 1.Dr. Dt. Neslihan Çökük. TAM SERAMİK SİSTEMLERİNE UYGULANAN FARKLI POLİSAJ METOTLARININ YÜZEY PÜRÜZLÜLÜĞÜNE ETKİSİNİN İNCELENMESİ. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi [Internet]. 2009 Feb. 1;2009(2):98-104. Available from: https://izlik.org/JA44PW26NH