THE EFFECT OF THREE DIFFERENT LUTING AGENT ON THE COMPRESSIF FRACTURE STRENGTH OF TURKOM CERATM ALL CERAMIC RESTORATIONS

Year 2008, Volume: 2008 Issue: 2, 47 - 52, 01.02.2008

Abstract

-

References

  • McLean JW. Evolution of dental ceramics in the twentieth century. J Prosthet Dent. 2001;85:61-6.
  • Chai J, Takahashi Y, Sulaiman F, Chong K, Lautenschlager EP. Probability of fracture of all- ceramic crowns. Int J Prosthodont. 2000;13:420-4.
  • Rosenblum MA, Schulman A. A review of all-ceramic restorations. J Am Dent Assoc. 1997;128:297-307.
  • Yavuzyılmaz H, Turhan B, Bavbek B, Kurt E. Tam porselen sistemleri II. Gazi Üni Dişhek Fak Derg. 2005;22:46-60.
  • Strub JR, Beschnidt SM. Fracture strength of 5 different all-ceramic crown systems. Int J Prosthodont. 1998;11:602-9.
  • Al-Makramani BM, Razak AA, Abu-Hassan MI. Effect of luting cements on the compressive strength of Turkom-Cera all-ceramic copings. J Contemp Dent Pract. 2008;9:33-40.
  • Yoshinari M, Derand T. Fracture strength of all- ceramic crowns. Int J Prosthodont. 1994;7:329-38.
  • Scherrer SS, de Rijk WG. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. Int J Prosthodont. 1993;6:462-7.
  • Philp GK, Brukl CE. Compressive strengths of conventional, twin foil, and all-ceramic crowns. J Prosthet Dent. 1984;52:215-20.
  • Sobrinho LC, Cattell MJ, Glover RH, Knowles JC. Investigation of the dry and wet fatigue properties of three all-ceramic crown systems. Int J Prosthodont. 1998;11:255-62.
  • Probster L. Survival rate of In-Ceram restorations. Int J Prosthodont. 1993;6:259-63.
  • Haselton DR, Diaz-Arnold AM, Hillis SL. Clinical assessment of high-strength all-ceramic crowns. J Prosthet Dent. 2000;83:396-401.
  • Lee SK, Wilson PR. Fracture strength of all-ceramic crowns with varying core elastic moduli. Aust Dent J. 2000;45:103-7.
  • White SN, Caputo AA, Vidjak FM, Seghi RR. Moduli of rupture of layered dental ceramics. Dent Mater. 1994;10:52-8.
  • Hwang JW, Yang JH. Fracture strength of copy- milled and conventional In-Ceram crowns. J Oral Rehabil. 2001;28:678-83.
  • Casson AM, Glyn Jones JC, Youngson CC, Wood DJ. The effect of luting media on the fracture resistance of a flame sprayed all-ceramic crown. J Dent. 2001;29:539-44.
  • Kelly JR. Clinically relevant approach to failure testing of all-ceramic restorations. J Prosthet Dent. 1999;81:652-61.
  • Esquivel-Upshaw JF, Chai J, Sansano S, Shonberg D. Resistance to staining, flexural strength, and chemical solubility of core porcelains for all-ceramic crowns. Int J Prosthodont. 2001;14:284-8.
  • McCormick JT, Rowland W, Shillingburg HT, Jr., Duncanson MG, Jr. Effect of luting media on the compressive strengths of two types of all-ceramic crown. Quintessence Int. 1993;24:405-8.

ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ

Year 2008, Volume: 2008 Issue: 2, 47 - 52, 01.02.2008

Abstract

Amaç: Bu çalışmada farklı simanların Turkom CeraTM tam seramik kronların kırılma dayanıklılığına olan etkisi araştırılmıştır. Metot: 30 adet ana güdük prepare edilmiş maksiller birinci premolar diş şeklinde üretilmiştir. 0,5mm kalınlığındaki 30 Turkom CeraTM koping üretilmiş ve kaplanmıştır. Üç tip siman materyali kullanılmıştır: Çinko Fosfat (Adhesor), Rezin Modifiye Cam İyonomer Siman (G CEM), ve Dual Cure Kompozit Rezin Siman (Clearfill Esthetic Cement). Her siman için 10 tam seramik kron simante edilmiştir. Tüm gruplar üretici talimatlarınca ve duyarlı yüklenme aygıtı kullanılarak 50 N’luk statik kuvvet altında simante edilmişlerdir. Tam seramik kronlar, üniversal test aygıtında başarısızlık gerçekleşene kadar (0,5 universal testing machine at a crosshead speed of 0.5 mm/dak) vertikal olarak yüklenmeye tabii tutulmuşlardır. mm/min until failure occurred. Bulgular: Gruplar arasında belirgin bir farklılık bulunmamıştır. Kırılma dayanıklılık testi sonuçları sırasıyla kompozit rezin siman için 1494 N, çinko fosfat siman için 1353 N, ve rezin modifiye cam iyonomer siman için 1777 N olarak bulunmuştur. Sonuçlar: Bu çalışmanın limitleri dahilinde, üç simantasyon ajanı Turkom CeraTM tam seramik kronların kırılma dayanıklılıklarına etki etmemektedir

References

  • McLean JW. Evolution of dental ceramics in the twentieth century. J Prosthet Dent. 2001;85:61-6.
  • Chai J, Takahashi Y, Sulaiman F, Chong K, Lautenschlager EP. Probability of fracture of all- ceramic crowns. Int J Prosthodont. 2000;13:420-4.
  • Rosenblum MA, Schulman A. A review of all-ceramic restorations. J Am Dent Assoc. 1997;128:297-307.
  • Yavuzyılmaz H, Turhan B, Bavbek B, Kurt E. Tam porselen sistemleri II. Gazi Üni Dişhek Fak Derg. 2005;22:46-60.
  • Strub JR, Beschnidt SM. Fracture strength of 5 different all-ceramic crown systems. Int J Prosthodont. 1998;11:602-9.
  • Al-Makramani BM, Razak AA, Abu-Hassan MI. Effect of luting cements on the compressive strength of Turkom-Cera all-ceramic copings. J Contemp Dent Pract. 2008;9:33-40.
  • Yoshinari M, Derand T. Fracture strength of all- ceramic crowns. Int J Prosthodont. 1994;7:329-38.
  • Scherrer SS, de Rijk WG. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. Int J Prosthodont. 1993;6:462-7.
  • Philp GK, Brukl CE. Compressive strengths of conventional, twin foil, and all-ceramic crowns. J Prosthet Dent. 1984;52:215-20.
  • Sobrinho LC, Cattell MJ, Glover RH, Knowles JC. Investigation of the dry and wet fatigue properties of three all-ceramic crown systems. Int J Prosthodont. 1998;11:255-62.
  • Probster L. Survival rate of In-Ceram restorations. Int J Prosthodont. 1993;6:259-63.
  • Haselton DR, Diaz-Arnold AM, Hillis SL. Clinical assessment of high-strength all-ceramic crowns. J Prosthet Dent. 2000;83:396-401.
  • Lee SK, Wilson PR. Fracture strength of all-ceramic crowns with varying core elastic moduli. Aust Dent J. 2000;45:103-7.
  • White SN, Caputo AA, Vidjak FM, Seghi RR. Moduli of rupture of layered dental ceramics. Dent Mater. 1994;10:52-8.
  • Hwang JW, Yang JH. Fracture strength of copy- milled and conventional In-Ceram crowns. J Oral Rehabil. 2001;28:678-83.
  • Casson AM, Glyn Jones JC, Youngson CC, Wood DJ. The effect of luting media on the fracture resistance of a flame sprayed all-ceramic crown. J Dent. 2001;29:539-44.
  • Kelly JR. Clinically relevant approach to failure testing of all-ceramic restorations. J Prosthet Dent. 1999;81:652-61.
  • Esquivel-Upshaw JF, Chai J, Sansano S, Shonberg D. Resistance to staining, flexural strength, and chemical solubility of core porcelains for all-ceramic crowns. Int J Prosthodont. 2001;14:284-8.
  • McCormick JT, Rowland W, Shillingburg HT, Jr., Duncanson MG, Jr. Effect of luting media on the compressive strengths of two types of all-ceramic crown. Quintessence Int. 1993;24:405-8.
There are 19 citations in total.

Details

Primary Language Turkish
Journal Section Articles
Authors

Yrd. Doç. Dr. Mustafa Zortürk This is me

Dt Filiz Yağcı This is me

Dt H. İbrahim Kılınç This is me

Dr H. Önder Gümüş This is me

Yrd. Doç. Dr. Süleyman Agüloğlu This is me

Publication Date February 1, 2008
Published in Issue Year 2008 Volume: 2008 Issue: 2

Cite

APA Zortürk, Y. D. D. M., Yağcı, D. F., Kılınç, D. H. İ., Gümüş, D. H. Ö., et al. (2008). ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi, 2008(2), 47-52.
AMA Zortürk YDDM, Yağcı DF, Kılınç DHİ, Gümüş DHÖ, Agüloğlu YDDS. ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ. Ata Diş Hek Fak Derg. February 2008;2008(2):47-52.
Chicago Zortürk, Yrd. Doç. Dr. Mustafa, Dt Filiz Yağcı, Dt H. İbrahim Kılınç, Dr H. Önder Gümüş, and Yrd. Doç. Dr. Süleyman Agüloğlu. “ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ”. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi 2008, no. 2 (February 2008): 47-52.
EndNote Zortürk YDDM, Yağcı DF, Kılınç DHİ, Gümüş DHÖ, Agüloğlu YDDS (February 1, 2008) ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi 2008 2 47–52.
IEEE Y. D. D. M. Zortürk, D. F. Yağcı, D. H. İ. Kılınç, D. H. Ö. Gümüş, and Y. D. D. S. Agüloğlu, “ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ”, Ata Diş Hek Fak Derg, vol. 2008, no. 2, pp. 47–52, 2008.
ISNAD Zortürk, Yrd. Doç. Dr. Mustafa et al. “ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ”. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi 2008/2 (February 2008), 47-52.
JAMA Zortürk YDDM, Yağcı DF, Kılınç DHİ, Gümüş DHÖ, Agüloğlu YDDS. ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ. Ata Diş Hek Fak Derg. 2008;2008:47–52.
MLA Zortürk, Yrd. Doç. Dr. Mustafa et al. “ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ”. Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi, vol. 2008, no. 2, 2008, pp. 47-52.
Vancouver Zortürk YDDM, Yağcı DF, Kılınç DHİ, Gümüş DHÖ, Agüloğlu YDDS. ÜÇ FARKLI SİMAN AJANININ TURKOM CERATM TAM SERAMİK KRONLARIN VERTİKAL KIRILMA DİRENCİ ÜZERİNE ETKİSİ. Ata Diş Hek Fak Derg. 2008;2008(2):47-52.

Bu eser Creative Commons Alıntı-GayriTicari-Türetilemez 4.0 Uluslararası Lisansı ile lisanslanmıştır. Tıklayınız.