The Connection Between Titanium Content, Bleaching and FR Protection of Wool

Year 2002, Volume: 4 Issue: 2 , 26 - 29 , 01.12.2002
https://izlik.org/JA86ML69YJ

Abstract

Potassium hexafluorotitanate was used for FR protection of wool (fibre and textile) in different conditions of treatment. Bleaching process was provided using of hydrogen peroxide and optical brightener bleaching system. The degree of FR protection was determined through the quantity of connected titanium in the wool. A modified procedure for the titanium determination in the wool using UV-vis spectrophotometry was developed. The connection between titanium content, bleaching and FR protection was established too

Year 2002, Volume: 4 Issue: 2 , 26 - 29 , 01.12.2002
https://izlik.org/JA86ML69YJ

Abstract

There are 0 citations in total.

Details

Other ID JA22DT79ES
Authors

Lj. Sinadinovska This is me

S. Ilievska This is me

İ. Spirevska This is me

J. Sinadinovski This is me

Submission Date December 1, 2002
Publication Date December 1, 2002
IZ https://izlik.org/JA86ML69YJ
Published in Issue Year 2002 Volume: 4 Issue: 2

Cite

APA Sinadinovska, L., Ilievska, S., Spirevska, İ., & Sinadinovski, J. (2002). The Connection Between Titanium Content, Bleaching and FR Protection of Wool. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi, 4(2), 26-29. https://izlik.org/JA86ML69YJ
AMA 1.Sinadinovska L, Ilievska S, Spirevska İ, Sinadinovski J. The Connection Between Titanium Content, Bleaching and FR Protection of Wool. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi. 2002;4(2):26-29. https://izlik.org/JA86ML69YJ
Chicago Sinadinovska, Lj., S. Ilievska, İ. Spirevska, and J. Sinadinovski. 2002. “The Connection Between Titanium Content, Bleaching and FR Protection of Wool”. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi 4 (2): 26-29. https://izlik.org/JA86ML69YJ.
EndNote Sinadinovska L, Ilievska S, Spirevska İ, Sinadinovski J (December 1, 2002) The Connection Between Titanium Content, Bleaching and FR Protection of Wool. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi 4 2 26–29.
IEEE [1]L. Sinadinovska, S. Ilievska, İ. Spirevska, and J. Sinadinovski, “The Connection Between Titanium Content, Bleaching and FR Protection of Wool”, Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi, vol. 4, no. 2, pp. 26–29, Dec. 2002, [Online]. Available: https://izlik.org/JA86ML69YJ
ISNAD Sinadinovska, Lj. - Ilievska, S. - Spirevska, İ. - Sinadinovski, J. “The Connection Between Titanium Content, Bleaching and FR Protection of Wool”. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi 4/2 (December 1, 2002): 26-29. https://izlik.org/JA86ML69YJ.
JAMA 1.Sinadinovska L, Ilievska S, Spirevska İ, Sinadinovski J. The Connection Between Titanium Content, Bleaching and FR Protection of Wool. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi. 2002;4:26–29.
MLA Sinadinovska, Lj., et al. “The Connection Between Titanium Content, Bleaching and FR Protection of Wool”. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi, vol. 4, no. 2, Dec. 2002, pp. 26-29, https://izlik.org/JA86ML69YJ.
Vancouver 1.Lj. Sinadinovska, S. Ilievska, İ. Spirevska, J. Sinadinovski. The Connection Between Titanium Content, Bleaching and FR Protection of Wool. Balıkesir Üniversitesi Fen Bilimleri Enstitüsü Dergisi [Internet]. 2002 Dec. 1;4(2):26-9. Available from: https://izlik.org/JA86ML69YJ