The dependence of some physical properties of corn cernel on moisture contents were determined. In samples, moisture contents were changed between 12.8 to 36.7 % as dry base (db). The lenght of grain were changed according to moisture centent, from 9.18 to 14.77 mm, the width from 5.63 to 10.30 mm, the thickness from 3.13 to 6.09 mm, volume of grain from 0.247 to 0.349 cm3, thousand grain mass from 226.30 to 314.56 g. porosity from 18.0 to 35.4%, projected area of grain from 1.345 to 1.775 cm². Friction coefficient of samples were determined for galvanized sheet metal, polywood and rubber surface. The largest value of coefficient friction was found on rubber. Bulk density decreased by increasing moisture contens from 871 to 656 kg/m³.
SELÇUK ÜNİVERSİTESİ
Dane mısırın farklı nem içeriğine göre bazı fiziksel özellikleri belirlenmiştir. Nem içeriği % 12.8... 36.7 arasında değişen örneklerin uzunluğu 9.18...14.77 mm, genişliği 5.63 ... 10.30 mm, kalınlığı 3.13 ... 6.09 mm, dane hacmi 0.247 ... 0.349 cm3, bin dane ağırlığı 226.30 ... 314.56 g, porozitesi % 18.0 ...35.4, dane izdüşüm alanı 1.345 ... 1.775 cm2'dır. Sürtünme katsayısı galvanizli sac, lastik ve kontraplak yüzeylerde belirlenmiştir. Sürtünme katsayısının en büyük değeri lastik yüzeyde or- taya çıkmıştır. Örneklerin hacım ağırlığı artan nem oranıyla 871 kg/m3'den 656 kg/ m³e düşmüştür.
SELÇUK ÜNİVERSİTESİ
Primary Language | English |
---|---|
Subjects | Cereals and Legumes |
Journal Section | Research Article |
Authors | |
Publication Date | December 31, 1996 |
Submission Date | January 5, 1996 |
Published in Issue | Year 1996 Volume: 10 Issue: 12 |
Selcuk Agricultural and Food Sciences is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License (CC BY NC).