Research Article
BibTex RIS Cite

A Study on Laser Processing of Ceramic Surface

Year 2019, Volume: 45 Issue: 1, 88 - 94, 30.04.2019

Abstract

In this study, laser processing processes of alumina
ceramics were investigated. The effect of laser power and processing speed on
alumina samples was investigated in this laser treatment procedure. The main
benefits of laser processing are flexibility, high speed, high precision and
good quality. In addition, ceramics are hardly processed by conventional
methods due to their high hardness and brittleness. CO2 laser
processing alumina ceramics were analyzed for the effect of output power,
process speed parameters. Mark width, sign depth, and contrast were evaluated
and the output power determined both the sign depth and width. Higher power,
resulting in deeper and wider markings characterized by high contrast. The
processing speed controls overlapping stains and the duration of the
laser-material interaction, thus having an effect on the depth and contrast of
the markers. The study explained that high output forces are required to
produce deep lines and that, with low processing speeds, high output forces become
clear as the most suitable parameters for achieving a satisfactory quality
width and depth during engraving. Samples were analyzed using a confocal
microscope and SEM.

References

  • Cervo, R., Ferro, P., & Tiziani, A. (2010). Annealing temperature effects on super duplex stainless steel UNS s32750 welded joints. I: Microstructure and partitioning of elements. Journal of Materials Science, 45(16), 4369–4377. http://doi.org/10.1007/s10853-010-4310-1Chen, M. F., Hsiao, W. T., Huang, W. L., Hu, C. W., & Chen, Y. P. (2009). Laser coding on the eggshell using pulsed-laser marking system. Journal of Materials Processing Technology, 209(2), 737–744. http://doi.org/10.1016/j.jmatprotec.2008.02.075Garino, J., Rahaman, M. N., & Bal, B. S. (2006). The Reliability of Modern Alumina Bearings in Total Hip Arthroplasty. Seminars in Arthroplasty, 17(3–4), 113–119. http://doi.org/10.1053/j.sart.2006.09.004Gómez De Salazar, J. M., Soria, A., & Barrena, M. I. (2007). The effect of N2 addition upon the MIG welding process of duplex steels. Journal of Materials Science, 42(13), 4892–4898. http://doi.org/10.1007/s10853-006-0557-yLeone, C., Lopresto, V., & De Iorio, I. (2009). Wood engraving by Q-switched diode-pumped frequency-doubled Nd:YAG green laser. Optics and Lasers in Engineering, 47(1), 161–168. http://doi.org/10.1016/j.optlaseng.2008.06.019Maleksaeedi, S., Eng, H., Wiria, F. E., Ha, T. M. H., & He, Z. (2014). Property enhancement of 3D-printed alumina ceramics using vacuum infiltration. Journal of Materials Processing Technology, 214(7), 1301–1306. http://doi.org/10.1016/j.jmatprotec.2014.01.019Migiakis, K., & Papadimitriou, G. D. (2009). Effect of nitrogen and nickel on the microstructure and mechanical properties of plasma welded UNS S32760 super-duplex stainless steels. Journal of Materials Science, 44(23), 6372–6383. http://doi.org/10.1007/s10853-009-3878-9Sorrentino, S., Fersini, M., & Zilli, G. (2009). Comparison between SAW and laser welding processes applied to duplex structures for bridges. Welding International, 23(9), 687–698. http://doi.org/10.1080/09507110902843214Turichin, G., Tsibulskiy, I., Kuznetsov, M., Akhmetov, A., Mildebrath, M., & Hassel, T. (2015). Influence of the Gap Width on the Geometry of the Welded Joint in Hybrid Laser-Arc Welding. Physics Procedia, 78(August), 14–23. http://doi.org/10.1016/j.phpro.2015.11.013Vogt, U. F., Gorbar, M., Dimopoulos-Eggenschwiler, P., Broenstrup, A., Wagner, G., & Colombo, P. (2010). Improving the properties of ceramic foams by a vacuum infiltration process. Journal of the European Ceramic Society, 30(15), 3005–3011. http://doi.org/10.1016/j.jeurceramsoc.2010.06.003
  • Chen, M. F., Hsiao, W. T., Huang, W. L., Hu, C. W., & Chen, Y. P. (2009). Laser coding on the eggshell using pulsed-laser marking system. Journal of Materials Processing Technology, 209(2), 737–744.
  • Garino, J., Rahaman, M. N., & Bal, B. S. (2006). The Reliability of Modern Alumina Bearings in Total Hip Arthroplasty. Seminars in Arthroplasty, 17(3–4), 113–119.
  • Gómez De Salazar, J. M., Soria, A., & Barrena, M. I. (2007). The effect of N2 addition upon the MIG welding process of duplex steels. Journal of Materials Science, 42(13), 4892–4898.
  • Leone, C., Lopresto, V., & De Iorio, I. (2009). Wood engraving by Q-switched diode-pumped frequency-doubled Nd:YAG green laser. Optics and Lasers in Engineering, 47(1), 161–168
  • Maleksaeedi, S., Eng, H., Wiria, F. E., Ha, T. M. H., & He, Z. (2014). Property enhancement of 3D-printed alumina ceramics using vacuum infiltration. Journal of Materials Processing Technology, 214(7), 1301–1306.
  • Migiakis, K., & Papadimitriou, G. D. (2009). Effect of nitrogen and nickel on the microstructure and mechanical properties of plasma welded UNS S32760 superstainless steels. Journal of Materials Science, 44(23), 6372–6383.
  • Sorrentino, S., Fersini, M., & Zilli, G. (2009). Comparison between SAW and laser welding processes applied to duplex structures for bridges. Welding International, 23(9), 687–698.
  • Turichin, G., Tsibulskiy, I., Kuznetsov, M., Akhmetov, A., Mildebrath, M., & Hassel, T. (2015). Influence of the Gap Width on the Geometry of the Welded Joint in Hybrid Laser-Arc Welding. Physics Procedia, 78(August), 14–23.
  • Vogt, U. F., Gorbar, M., Dimopoulos-Eggenschwiler, P., Broenstrup, A., Wagner, G., & Colombo, P. (2010). Improving the properties of ceramic foams by a vacuum infiltration process. Journal of the European Ceramic Society, 30(15), 3005–3011.

Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma

Year 2019, Volume: 45 Issue: 1, 88 - 94, 30.04.2019

Abstract

Bu çalışmada, alümina
seramiklerinin lazerle işleme süreçleri araştırılmıştır. Bu lazer işleme
prosedüründe lazer gücü ve işlem hızının alümina örnekleri üzerindeki etkisi
incelenmiştir. Lazer işlemenin başlıca faydaları esneklik ile birlikte yüksek
hız, yüksek hassasiyet ve iyi kalitedir. Ayrıca, seramikler yüksek sertlikleri
ve kırılganlıkları nedeniyle geleneksel yöntemlerle zorlukla işlenir. CO2
lazer işleme alümina seramiklerinin, çıkış gücü, işlem hızı parametrelerinin
etkisi ile ilgili analizleri yapıldı. İşaret genişliği, işaret derinliği ve
kontrast değerlendirildi ve çıktı gücünün hem işaret derinliğini hem de
genişliği belirlediği tespit edildi. Daha yüksek güç, yüksek kontrast ile
karakterize edilmiş, bu durum daha derin ve daha geniş işaretlerin oluşmasına
neden olmuştur. İşlem hızı, üst üste binen lekeleri ve lazer-malzeme etkileşim
süresini kontrol eder, böylece işaret derinliği ve kontrastı üzerinde etkisi
olur. Araştırma, derin çizgiler üretmek için yüksek çıkış güçlerinin gerekli
olduğunu ve düşük işlem hızlarıyla birlikte yüksek çıkış güçlerinin, gravürleme
sırasında tatmin edici kalitede genişliği ve derinliği elde etmek için en uygun
parametreler olduğu neticesinde netleştiğini açıkladı. Örnekler konfokal
mikroskop ve SEM kullanılarak analiz edildi.

References

  • Cervo, R., Ferro, P., & Tiziani, A. (2010). Annealing temperature effects on super duplex stainless steel UNS s32750 welded joints. I: Microstructure and partitioning of elements. Journal of Materials Science, 45(16), 4369–4377. http://doi.org/10.1007/s10853-010-4310-1Chen, M. F., Hsiao, W. T., Huang, W. L., Hu, C. W., & Chen, Y. P. (2009). Laser coding on the eggshell using pulsed-laser marking system. Journal of Materials Processing Technology, 209(2), 737–744. http://doi.org/10.1016/j.jmatprotec.2008.02.075Garino, J., Rahaman, M. N., & Bal, B. S. (2006). The Reliability of Modern Alumina Bearings in Total Hip Arthroplasty. Seminars in Arthroplasty, 17(3–4), 113–119. http://doi.org/10.1053/j.sart.2006.09.004Gómez De Salazar, J. M., Soria, A., & Barrena, M. I. (2007). The effect of N2 addition upon the MIG welding process of duplex steels. Journal of Materials Science, 42(13), 4892–4898. http://doi.org/10.1007/s10853-006-0557-yLeone, C., Lopresto, V., & De Iorio, I. (2009). Wood engraving by Q-switched diode-pumped frequency-doubled Nd:YAG green laser. Optics and Lasers in Engineering, 47(1), 161–168. http://doi.org/10.1016/j.optlaseng.2008.06.019Maleksaeedi, S., Eng, H., Wiria, F. E., Ha, T. M. H., & He, Z. (2014). Property enhancement of 3D-printed alumina ceramics using vacuum infiltration. Journal of Materials Processing Technology, 214(7), 1301–1306. http://doi.org/10.1016/j.jmatprotec.2014.01.019Migiakis, K., & Papadimitriou, G. D. (2009). Effect of nitrogen and nickel on the microstructure and mechanical properties of plasma welded UNS S32760 super-duplex stainless steels. Journal of Materials Science, 44(23), 6372–6383. http://doi.org/10.1007/s10853-009-3878-9Sorrentino, S., Fersini, M., & Zilli, G. (2009). Comparison between SAW and laser welding processes applied to duplex structures for bridges. Welding International, 23(9), 687–698. http://doi.org/10.1080/09507110902843214Turichin, G., Tsibulskiy, I., Kuznetsov, M., Akhmetov, A., Mildebrath, M., & Hassel, T. (2015). Influence of the Gap Width on the Geometry of the Welded Joint in Hybrid Laser-Arc Welding. Physics Procedia, 78(August), 14–23. http://doi.org/10.1016/j.phpro.2015.11.013Vogt, U. F., Gorbar, M., Dimopoulos-Eggenschwiler, P., Broenstrup, A., Wagner, G., & Colombo, P. (2010). Improving the properties of ceramic foams by a vacuum infiltration process. Journal of the European Ceramic Society, 30(15), 3005–3011. http://doi.org/10.1016/j.jeurceramsoc.2010.06.003
  • Chen, M. F., Hsiao, W. T., Huang, W. L., Hu, C. W., & Chen, Y. P. (2009). Laser coding on the eggshell using pulsed-laser marking system. Journal of Materials Processing Technology, 209(2), 737–744.
  • Garino, J., Rahaman, M. N., & Bal, B. S. (2006). The Reliability of Modern Alumina Bearings in Total Hip Arthroplasty. Seminars in Arthroplasty, 17(3–4), 113–119.
  • Gómez De Salazar, J. M., Soria, A., & Barrena, M. I. (2007). The effect of N2 addition upon the MIG welding process of duplex steels. Journal of Materials Science, 42(13), 4892–4898.
  • Leone, C., Lopresto, V., & De Iorio, I. (2009). Wood engraving by Q-switched diode-pumped frequency-doubled Nd:YAG green laser. Optics and Lasers in Engineering, 47(1), 161–168
  • Maleksaeedi, S., Eng, H., Wiria, F. E., Ha, T. M. H., & He, Z. (2014). Property enhancement of 3D-printed alumina ceramics using vacuum infiltration. Journal of Materials Processing Technology, 214(7), 1301–1306.
  • Migiakis, K., & Papadimitriou, G. D. (2009). Effect of nitrogen and nickel on the microstructure and mechanical properties of plasma welded UNS S32760 superstainless steels. Journal of Materials Science, 44(23), 6372–6383.
  • Sorrentino, S., Fersini, M., & Zilli, G. (2009). Comparison between SAW and laser welding processes applied to duplex structures for bridges. Welding International, 23(9), 687–698.
  • Turichin, G., Tsibulskiy, I., Kuznetsov, M., Akhmetov, A., Mildebrath, M., & Hassel, T. (2015). Influence of the Gap Width on the Geometry of the Welded Joint in Hybrid Laser-Arc Welding. Physics Procedia, 78(August), 14–23.
  • Vogt, U. F., Gorbar, M., Dimopoulos-Eggenschwiler, P., Broenstrup, A., Wagner, G., & Colombo, P. (2010). Improving the properties of ceramic foams by a vacuum infiltration process. Journal of the European Ceramic Society, 30(15), 3005–3011.
There are 10 citations in total.

Details

Primary Language Turkish
Journal Section Research Articles
Authors

Mehmet Hakan Çolpan

Publication Date April 30, 2019
Submission Date April 1, 2019
Published in Issue Year 2019 Volume: 45 Issue: 1

Cite

APA Çolpan, M. H. (2019). Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma. Selçuk Üniversitesi Fen Fakültesi Fen Dergisi, 45(1), 88-94.
AMA Çolpan MH. Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma. sufefd. April 2019;45(1):88-94.
Chicago Çolpan, Mehmet Hakan. “Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma”. Selçuk Üniversitesi Fen Fakültesi Fen Dergisi 45, no. 1 (April 2019): 88-94.
EndNote Çolpan MH (April 1, 2019) Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma. Selçuk Üniversitesi Fen Fakültesi Fen Dergisi 45 1 88–94.
IEEE M. H. Çolpan, “Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma”, sufefd, vol. 45, no. 1, pp. 88–94, 2019.
ISNAD Çolpan, Mehmet Hakan. “Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma”. Selçuk Üniversitesi Fen Fakültesi Fen Dergisi 45/1 (April 2019), 88-94.
JAMA Çolpan MH. Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma. sufefd. 2019;45:88–94.
MLA Çolpan, Mehmet Hakan. “Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma”. Selçuk Üniversitesi Fen Fakültesi Fen Dergisi, vol. 45, no. 1, 2019, pp. 88-94.
Vancouver Çolpan MH. Seramik Yüzeylerin Lazerle İşlenmesi Üzerine Bir Çalışma. sufefd. 2019;45(1):88-94.

Journal Owner: On behalf of Selçuk University Faculty of Science, Rector Prof. Dr. Hüseyin YILMAZ
Selcuk University Journal of Science Faculty accepts articles in Turkish and English with original results in basic sciences and other applied sciences. The journal may also include compilations containing current innovations.

It was first published in 1981 as "S.Ü. Fen-Edebiyat Fakültesi Dergisi" and was published under this name until 1984 (Number 1-4).
In 1984, its name was changed to "S.Ü. Fen-Edeb. Fak. Fen Dergisi" and it was published under this name as of the 5th issue.
When the Faculty of Letters and Sciences was separated into the Faculty of Science and the Faculty of Letters with the decision of the Council of Ministers numbered 2008/4344 published in the Official Gazette dated 3 December 2008 and numbered 27073, it has been published as "Selcuk University Journal of Science Faculty" since 2009.
It has been scanned in DergiPark since 2016.

88x31.png

Selcuk University Journal of Science Faculty is licensed under a Creative Commons Attribution-NonCommercial 4.0 International (CC BY-NC 4.0) License.