In this study, the representative samples were taken from the halloysite deposits located in Çanakkale-Balıkesir regions, in NW Anatolia. At first, the dehydration temperatures of the samples were determined after sample preparation and characterization studies. It was found that halloysite samples began to lose their interlayer waters at 50°C and continued up to 70°C. The intercalation studies were carried out on dehydrated samples by using ethylene glycol, potassium acetate, dimethyl sulfoxide and formamide. Although there were negative results by ethylene glycol and potassium acetate, the satisfactory results were obtained by dimethyl sulfoxide and formamide. It was understood that the most effective reagent in terms of intercalation was formamide.
Intercalation Halloysite Kaolinite Dimethyl Sulfoxide Formamide.
Birincil Dil | İngilizce |
---|---|
Konular | Mühendislik |
Bölüm | Makaleler |
Yazarlar | |
Yayımlanma Tarihi | 30 Haziran 2015 |
Yayımlandığı Sayı | Yıl 2015 Cilt: 150 Sayı: 150 |
Copyright and Licence
The Bulletin of Mineral Research and Exploration keeps the Law on Intellectual and Artistic Works No: 5846. The Bulletin of Mineral Research and Exploration publishes the articles under the terms of “Creatice Common Attribution-NonCommercial-NoDerivs (CC-BY-NC-ND 4.0)” licence which allows to others to download your works and share them with others as long as they credit you, but they can’t change them in any way or use them commercially.
For further details;
https://creativecommons.org/licenses/?lang=en