Inconel 625 AISI 304L paslanmaz çelik Mikroyapı Sertlik Tokluk
In this study, a couple of Inconel 625 nickel based super alloy and AISI 304 L austenitic stainless steel dissimilar materials were welded by TIG (gas tungsten arc welding) method using ErNiCr3 filler metal. A couple of dissimilar materials with different physical and chemical properties are joined with a high nickel content filler metal, and the weld metal microstructure, hardness and toughness properties of the weld are investigated. Microstructural transformations and intermetallic phases in the weld metal and at the melting boundary and precipitates formed in the structure have been characterized. Microstructural changes, which depend on the chemical composition of base metal are examined both in terms of weld metal and HAZ (Heat Affected Zone). Depending on the dilution amount, the difference in weld metal and HAZ chemical concentration was determined by SEM / EDS (Scanning Electron Microscopy/Energy Dispersive Spectroscopy) assistance mapping process. The obtained weld metal has high toughness properties at low temperatures. The chemical content of weld metal has exposed to partial elemental changes due to dilution.
Inconel 625 AISI 304L stainless steel Microstructure Hardness Toughness
Birincil Dil | Türkçe |
---|---|
Bölüm | Makaleler |
Yazarlar | |
Yayımlanma Tarihi | 30 Haziran 2018 |
Yayımlandığı Sayı | Yıl 2018 Cilt: 33 Sayı: 2 |