Öz

In this study, the effects of polyamide-6,6 (PA 66) nanofibers on the free vibration and torsional buckling of four-layered E-glass/epoxy composite drive shaft were investigated numerically. The numerical analyses were carried out by using ANSYS 16.2 software package. Three different nanofiber areal weight densities (AWDs), 8, 10 and 12 g/m2, were considered to reveal the relationship between the amount of nanofibers in the interlaminar region and natural frequencies/critical torsional buckling loads. The numerical results showed that the PA-66 nanofibers had a positive effect on natural frequencies and torsional buckling load of E-glass/epoxy composite shaft. The natural frequencies and buckling load of the composite shaft can be increased by about 10 % and 22% using PA 66 nanofibers as the secondary reinforcing material in the interlaminar region. The failure torque values were not significantly affected with the inclusion of PA 66 nanofibers in the interlaminar region.

Anahtar Kelimeler

Kaynakça

  1. [1] Greenhalgh, E.S., Rogers, C., Robinson, P. 2009. Fractographic observations on delamination growth and the subsequent migration through the laminate. Composites Science and Technology, Cilt. 69(14), s. 2345-2351.DOI:10.1016/j.compscitech.2009.01.034
  2. [2] Greenhalgh E.S. 2009. Failure analysis and fractography of polymer composites, CRC Press.
  3. [3] Beylergil, B., Tanoglu, M., Aktaş, E. 2017. Enhancement of interlaminar fracture toughness of carbon fiber/epoxy composites using polyamide 6/6 electrospun nanofibers. Journal of Applied Polymer Science, Cilt. 134(35): 45244. DOI: 10.1002/app.45244
  4. [4] Daelemans, L., van der Heijden, S., De Baere I, Rahier H, Van Paepegem, W., De Clerck, K.2015. Nanofibre bridging as a toughening mechanism in carbon/epoxy composite laminates interleaved with electrospun polyamide nanofibrous veils. Composites Science and Technology, Cilt. 117, s.244–256. DOI: 10.1016/j.compscitech.2015.06.021
  5. [5] Zhang, H., Bharti, A., Li, Z., Du, S., Bilotti, E., Peijs, T. 2015. Localized toughening of carbon/ epoxy laminates using dissolvable thermoplastic interleaves and electrospun fibres. Composites Part A: Applied Science and Manufacturing, Cilt. 79: s. 116–26 DOI:10.1016/j.compositesa.2015.09.024
  6. [6] Li, G., Li, P., Yu, Y., Jia, X., Zhang, S., Yang, X., Ryu, S. 2008. Novel carbon fiber/epoxy composite toughened by electrospun polysulfone nanofibers. Materials Letters, Cilt.62(3), s. 511–514. DOI: 10.1016/j.matlet.2007.05.080
  7. [7] Li, G., Li, P., Zhang, C., Yu, Y., Liu, H., Zhang, S., Jia, X., Yang, X., Xue, Z., Ryu, S. 2008. Inhomogeneous toughening of carbon fiber/epoxy composite using electrospun polysulfone nanofibrous membranes by in situ phase separation. Composites Science Technology Cilt.68(3–4)i s. 987–94. DOI: 10.1016/j.compscitech.2007.07.010
  8. [8] Saghafi, H., Brugo, T., Minak, G., Zucchelli, A. 2015. The effect of PVDF nanofibers on mode-I fracture toughness of composite materials. Composites Part B: Engineering, Cilt.72, s. 213–216. DOI:10.1016/j.compositesb.2014.12.015

Ayrıntılar

Birincil Dil

İngilizce

Konular

Mühendislik

Bölüm

Araştırma Makalesi

Yayımlanma Tarihi

15 Eylül 2018

Gönderilme Tarihi

24 Nisan 2018

Kabul Tarihi

26 Haziran 2018

Yayımlandığı Sayı

Yıl 2018 Cilt: 20 Sayı: 60

Kaynak Göster

APA
Beylergil, B. (2018). Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers. Dokuz Eylül Üniversitesi Mühendislik Fakültesi Fen ve Mühendislik Dergisi, 20(60), 1036-1044. https://izlik.org/JA55SY48XA
AMA
1.Beylergil B. Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers. DEUFMD. 2018;20(60):1036-1044. https://izlik.org/JA55SY48XA
Chicago
Beylergil, Bertan. 2018. “Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers”. Dokuz Eylül Üniversitesi Mühendislik Fakültesi Fen ve Mühendislik Dergisi 20 (60): 1036-44. https://izlik.org/JA55SY48XA.
EndNote
Beylergil B (01 Eylül 2018) Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers. Dokuz Eylül Üniversitesi Mühendislik Fakültesi Fen ve Mühendislik Dergisi 20 60 1036–1044.
IEEE
[1]B. Beylergil, “Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers”, DEUFMD, c. 20, sy 60, ss. 1036–1044, Eyl. 2018, [çevrimiçi]. Erişim adresi: https://izlik.org/JA55SY48XA
ISNAD
Beylergil, Bertan. “Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers”. Dokuz Eylül Üniversitesi Mühendislik Fakültesi Fen ve Mühendislik Dergisi 20/60 (01 Eylül 2018): 1036-1044. https://izlik.org/JA55SY48XA.
JAMA
1.Beylergil B. Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers. DEUFMD. 2018;20:1036–1044.
MLA
Beylergil, Bertan. “Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers”. Dokuz Eylül Üniversitesi Mühendislik Fakültesi Fen ve Mühendislik Dergisi, c. 20, sy 60, Eylül 2018, ss. 1036-44, https://izlik.org/JA55SY48XA.
Vancouver
1.Bertan Beylergil. Free Vibration and Torsional Buckling Analysis of E- Glass/Epoxy Composite Shafts with Polyamide-6,6 (PA 66) Nanofiber Interlayers. DEUFMD [Internet]. 01 Eylül 2018;20(60):1036-44. Erişim adresi: https://izlik.org/JA55SY48XA

Bu dergi, Creative Commons Atıf-GayriTicari 4.0 Uluslararası Lisansı (CC BY-NC 4.0) altında lisanslanmıştır.

download?token=eyJhdXRoX3JvbGVzIjpbXSwiZW5kcG9pbnQiOiJmaWxlIiwicGF0aCI6IjliNTAvMDBjMi8xZmIxLzY5MjZmZDIyOGE1NzgyLjA3MzU5MTk2LnBuZyIsImV4cCI6MTc2NDE2OTE1Nywibm9uY2UiOiJhZDRmNjNlNzdhOWYwOWQ4YTNjNGVmNGIxOTFlZWViNyJ9.4Dxgc9mc-p4Tyti8NTU5pxEfGUWeuJud1fPWxu2mUy8